ASTM F
392/F 392M Standard Practice for Conditioning Flexible Barrier Materials for Flex Durability 软性屏障材料抗揉搓性的标准试验方法 |
|
Condition A—Full cycle conditions for 1 h at 45 cpm (2700 cycles),评估方式需要另外收费,测试后确认 |
|
Condition B—Full cycle for 20 min at 45 cpm (900 cycles).评估方式需要另外收费,测试后确认 |
|
Condition C—Full cycle conditions for 6 min at 45 cpm (270 cycles).评估方式需要另外收费,测试后确认 |
|
Condition D—Full cycle for approximately 1⁄2 min at 45 cpm (20 cycles).评估方式需要另外收费,测试后确认 |
| Condition E—部分循环 20 cycles at 45 cpm.评估方式需要另外收费,测试后确认 |
| 送样规格 sample size: 20个成品 , 20pcs x 300 x 350mm |
| 测试周期 Lead time: 9 working days |